Carbon Nanotube-Polystyrene Microspheres Prepared by Electrostatic Adsorption, CNTs: 25 wt%; Polystyrene Microspheres: 75 wt%

Brands:MOLCHEM

162.00748.00

Clear

Description

Carbon Nanotube-Polystyrene Microspheres Prepared by Electrostatic Adsorption

CNTs: 25 wt%, Polystyrene Microspheres: 75 wt%

Technical Properties:

Carbon Nanotubes
Purity > 95 wt%
Outside Diameter (nm) > 50
Inside Diameter (nm) 5.0-15.0
Length (μm) 5.0-20.0
Manufacturing Method CVD
Color black
Polystyrene Microspheres
Average Particle Size (nm) 100-300
Shape spherical
CNTs 20 wt%; Polystyrene Microspheres 80 wt%
Specific Surface Area (m2/g) 8
Volume Resistivity (Ω.cm) <10
Volume Resistivity Content Relationship
CNTs Content wt% 0.00 6.00 12.00 15.00 20.00 25.00
Volume Resistivity (Ω·cm) >2.0E06 4.0E05 95.30 28.20 7.00 4.00

Applications:

Polystyrene surface is usually negatively charged. Carbon nanotubes are treated with cationic surfactant (Cetyl trimethyl ammonium bromide).
Carbon nanotubes and polystyrene self assemble to form a uniform stable complex. The complex shows high strength and conductivity which makes
it suitable for processing into conductive plastics, conductive sheets, and films.

Brand

MOLCHEM

Additional information

Quantity

5 g, 25 g, 100 g

Reviews

There are no reviews yet.

Be the first to review “Carbon Nanotube-Polystyrene Microspheres Prepared by Electrostatic Adsorption, CNTs: 25 wt%; Polystyrene Microspheres: 75 wt%”